How feasable is stamping your own pots with lips from thin alu?

Discussion in 'Fettling Forum' started by TRA_A, Jan 23, 2022.

  1. TRA_A Israel

    Offline
    Joined:
    Jul 29, 2020
    Messages:
    285
    Location:
    NI
    How feasable is stamping your own pots with lips* from thin alu? In the absence of much expensive equipment that is..

    Eg if you wanted to make a hyperUL third inner pot for a trangia (ie an inner-inner pot :) ).

    * for the pot grabber to grip on.
     
  2. Ian

    Ian Subscriber

    Offline
    Joined:
    Jul 26, 2004
    Messages:
    7,113
    Location:
    West Yorkshire
    Do you need to?
    I think most pot lifters grip the pot wall rather than the lip, but they have to be able to accommodate the lip to do so.
    Also, if you're aiming for 'hyperUL', you might look at the GSI Minimalist pot grabber, (<½oz).
     
  3. Odd

    Offline
    Joined:
    Oct 4, 2013
    Messages:
    737
    Location:
    Östhammar, Sweden
    I'd recommend pressure spinning it - only needs a hardwood original form to build the form of the sheet metal disc against in your lathe.
    That's the way lots of thinwall round things are made.
    /Odd
     
  4. SveaSizzler

    SveaSizzler United States Subscriber

    Offline
    Joined:
    Jul 26, 2016
    Messages:
    2,208
    Location:
    Tucson, Arizona
    Would one of the T-27 pots nest inside the T-25 set?
     
  5. TRA_A Israel

    Offline
    Joined:
    Jul 29, 2020
    Messages:
    285
    Location:
    NI
    Yes, but you would need a pan stand or crosspiece.

    Also, it was the mainly the 27 I was thinking of.
     
  6. TRA_A Israel

    Offline
    Joined:
    Jul 29, 2020
    Messages:
    285
    Location:
    NI
    Thanks, but I don't have a lathe.
     
  7. TRA_A Israel

    Offline
    Joined:
    Jul 29, 2020
    Messages:
    285
    Location:
    NI
    I had assumed the pot gripping was made more secure by the lip having lost dinner on the v1 duossals' less substantial lip cf plain alu 27 pots.
     
  8. Scrambler

    Scrambler Australia Subscriber

    Offline
    Joined:
    Jan 29, 2013
    Messages:
    1,146
    Location:
    Australia
    The pot from one of these does exactly what you want:

    Sportztrek Hard Anodised Trek Set - 5 Piece

    They are an Australian brand, but I assume a Chinese item available through other brands in other places.

    The pot is slightly narrower, but squarer in the corners compared to the smaller T27 pot. The height inserted works.

    The squarer profile means there is a small gap under the pot when used as the third in a T27. The contact is the bottom edge. Still, does what you need. Burner and gripper fit.

    I don't have UL to compare. The Sportztrek pot weighs 70g. It is hard anodised. My older T27 pots weigh just over 100g.
     
  9. TRA_A Israel

    Offline
    Joined:
    Jul 29, 2020
    Messages:
    285
    Location:
    NI
    Thanks
     
  10. Gunner

    Offline
    Joined:
    Mar 16, 2018
    Messages:
    421
    @TRA_A
    I think it likely that you'd need to anneal (soften) the alu sheet to make it ductile enough to form without cracking, as that metal work hardens quite rapidly - i.e., if you put it under any stress, by bending, twisting, hammering, etc, it gets harder and harder until any further stress will make it crack.

    Almost certainly, it won't be pure aluminium, but an alloy of aluminium with one or more of copper, magnesium, manganese, silicon, tin or zinc. The mix has a marked effect on the properties, and unless you know the composition and grade, the simplest way to check is to bend it into a fairly sharp radius and see what happens. If it bends without apparent cracking, but the surface on the outside of the bend looks rather white, it needs annealing. The white appearance is actually a myriad of tiny surface cracks; if you see them, the metal is too close to cracking for comfort - especially if it will have boiling water inside it!

    Be warned that some Aluminium alloys - such as those alloyed with copper and zinc - are so fussy that you need an industrial grade annealing oven, and maybe a timer which can control the rate of cooling to 50 degrees F per hour. And both are very prone to stress-cracking!

    Light alloys used to make pots and pans are commonly Aluminium Manganese alloys. These are very formable, and anneal fairly easily.
    Aluminium Magnesium and Aluminium Magnesium Silicon alloys are commonly found in sheet form, can be worked fairly easily, and are pretty easy to anneal.

    A home workshop way of annealing these alloys only needs a source of heat and a bar of soap. Smear thin lines of soap on the top surface, then heat the alloy as evenly as possible on the underside until the soap turns brown. Leave to cool down naturally - don't quench in water. Annealing temperatures range from 650 - 775 degrees F, depending on grade. This is getting pretty close to melting points, so take great care to heat evenly, avoiding the creation of hot-spots.

    Depending on the amount of bending / stretching, you may need to do it in stages, stopping short as soon as your feel the metal getting hard, and re-annealing before working it some more.

    HTH,